♦ Quenched Heat treatment at Temp.860-900 Deg.C and Tempered treatment at 620-680 Deg.C
♦ Flattening test according to EN 10233
♦ Ring Tensile test comply to EN 10237
♦ Impacting test comply to EN 10045-1
♦ Issued Orginal Mill test certificate under EN10204 3.1/3.2 FORMAT
♦ Surface Protection:Black,Varnish,Hot Dip Galvanized,Coating with shop prime
►Mechnical property for 25CrMo4 boiler steel pipes:
|
25CrMo4 |
||||
|
Yield strength (≥Mpa) |
T≤16 |
16<T≤40 |
40<T≤60 |
60<T≤100 |
|
355 |
355 |
355 |
- |
|
|
Tensile strength (≥Mpa) |
540-680 |
|||
►Chemical composition for 25CrMo4 Boiler steel pipes (Heat Analysis Max%)
|
Main chemical elements composition of 25CrMo4 |
||||
|
C |
Si |
Mn |
P |
S |
|
0.22-0.29 |
0.40 |
0.60-0.90 |
0.025 |
0.020 |
|
Cr |
Mo |
Ni |
Alt |
Cu |
|
0.9-1.2 |
0.15-0.30 |
0.30 |
0.04 |
0.30 |
+86 371 55057610
inquiry@xsteelplate.com







Tel:+86 371 55057610