♦ Ultrasonic test according to ASTM A578,A577 or A435
♦ Definiations for Mechanical testing comply to A370
♦ Test Methods,Practices and Terminology for chemical analysis comply to A751
♦ Practices for detecting susceptibility to Intergranular corrosion in Austenitic stainless steels
♦ Packing with water-resistance paper and Non-fumigation wooden crates
♦ Paper Interleave,Polyethylene Film coating (PE COAT)for cold rolled stainless steels
►Mechnical property for Stainless sheet A240 TP 431
|
Stainless steel plate A240 431 |
||||
|
Yield strength (≥Mpa) |
Tensile strength (≥Mpa) |
Elogation in 50mm min. % |
Hardness, Max |
|
|
Brinell HBW |
Rockwell HRC |
|||
|
- |
- | - | 285 |
29 |
►Chemical composition for Stainless sheet A240 TP 431 (Heat Analysis Max%)
|
Main chemical elements composition of Stainless steel plate A240 431 |
|||||
|
C |
Mn |
P |
S |
Si |
Cr |
|
0.20 |
1.0 |
0.040 |
0.030 |
1.0 |
15-17 |
|
Ni |
N |
Al |
Ti |
Al |
Cu |
|
1.25-2.50 |
- |
- |
- |
- |
- |
+86 371 55057610